Zum Hauptinhalt springen

Field cards for common bead problems

Recall first checks for four common bead problems without jumping to a random fix.

welding-fundamentals4 min read

Porosity It is just a few pinholes; grind and keep going. Visible porosity appears on a repeated bead. Your line I am stopping the repeat and checking shielding, wind, nozzle, gas path, moisture, and base-metal cleanliness before the next bead. Grinding evidence away before checking the process condition. Porosity often points upstream; stopping protects the batch. Undercut Undercut at the toe: reflex or move? Undercut is a geometry and heat-control clue, not a universal call for more heat. Lack of fusion First checks when the bead sits on the sidewall? Joint access, clean surface, work angle, travel speed, heat setting,…

Read the full lesson

Sign up free: one personalized lesson every day, matched to your role and goals.

← Back to library

Kontakt aufnehmen